Detail of Operations – Welding Procedure Part Number: ANC-20643WLD Number 1
Operation/Description Prepare weld joint. Clean the area of all foreign material
2
Confirm that the filler wire is compatible with the base material
3
Use GMAW process
4
Pre heat parts to 150 degrees F
5
Tack weld in four (4) places alternating the tacks 180 degrees opposed
6
Apply the first bead in quadrants to maintain concentricity. Inspect upon completion
7
Apply subsequent beads. Maximum interpass temperature to be less than 750 degrees F. Inspect each completed bead.
8
Apply finish cap over completed beads. Blend the cap into the base metal.
9
Remove all slag and weld spatter
Ref. Specs. P8A-AG1 ANC-20643
Equipment Miller Syncrowave 200